Low-pressure plasma treatments in an rf discharge of O-2 and Ar were employed to introduce polar functional groups onto the biaxial-oriented polypropylene (BOPP) surfaces to enhance the wettability and activation. The effects of plasma treatment on the morphology and wettability of the BOPP films were characterized using static contact angle measurements, attenuated total reflection (ATR)-FTIR spectroscopy, scanning electron microscopy (SEM) and atomic force microscopy (AFM). A clear increase in the surface energy of BOPP films due to O-2 and Ar plasma treatments was observed. The surfaces became highly hydrophilic when exposed for 20 s or longer to the plasma discharge. The wettability of polymer surface can be improved when oxygen functionalities are generated, which can be achieved directly in O-containing plasmas or via post plasma reactions. Small reduction in surface energy of plasma treated BOPP films, after 30 days aging showed that the plasma-induced cross-linking in BOPP film was not the dominant phenomena. With increasing the treatment power and time, rate of the decrease in surface energy after aging is reduced. AFM and SEM images revealed distinct changes in the topography of BOPP due to O-2 and Ar plasma treatments. Nodular structure is formed on the BOPP film during the treatment and the size of the nodules increases with the treatment time. (c) 2007 Published by Elsevier B.V.
机译:在O-2和Ar的射频放电中进行低压等离子体处理,将极性官能团引入双轴取向聚丙烯(BOPP)表面,以增强润湿性和活化性。使用静态接触角测量,衰减全反射(ATR)-FTIR光谱,扫描电子显微镜(SEM)和原子力显微镜(AFM)表征了等离子体处理对BOPP膜的形貌和润湿性的影响。观察到由于O-2和Ar等离子处理,BOPP膜的表面能明显增加。当暴露于等离子体放电20秒或更长时间时,表面变得高度亲水。当产生氧官能团时,可以改善聚合物表面的润湿性,这可以直接在含O的等离子体中或通过后等离子体反应实现。老化30天后,等离子体处理过的BOPP薄膜的表面能略有下降,这表明BOPP薄膜中等离子体诱导的交联不是主要现象。随着处理能力和时间的增加,老化后表面能的降低速率降低。 AFM和SEM图像显示,由于O-2和Ar等离子体处理,BOPP的形貌发生了明显变化。在处理期间,BOPP膜上形成结节结构,并且结节的尺寸随处理时间的增加而增加。 (c)2007年由Elsevier B.V.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号