In this, the first report of precision and accuracy in simulator studies, ceramic-ceramic implants with ultra-low wear trends represented a relevant wear model. The effect of test durations was examined in a standard simulator test mode on the quality of the linear regression trends, the average wear estimates, and the amount of noise in the data. Three sets of diametral tolerances were compared in 28 mm diameter alumina implants. The authors' hypothesis was that wear data would be significantly improved with increased test durations. The average wear rates varied little with test duration, the biggest change amounting to only 30 and 15 per cent decreases in the wear estimate by 10 and 14 million cycles respectively. The most satisfactory improvement in the study was the decrease in variance (noise) with increasing duration, ±200 per cent at 5 million cycles reduced to ±55 per cent at 14 million cycles. The quality of the linear regression coefficients improved 150 per cent by 10 million cycles and 250 per cent by 14 million cycles. Overall the ceramic implants with highest diametral tolerances showed the least wear (15 per cent less, but not statistically significant). However, given such low wear rates for alumina liners, it was unlikely that any differences owing to diametral tolerances would be clinically significant in the typical patient.
机译:在这是模拟器研究的精度和准确性的第一份报告中,具有超低磨损趋势的陶瓷陶瓷植入物代表了一种相关的磨损模型。在标准模拟器测试模式下,检查了测试持续时间对线性回归趋势的质量,平均磨损估算值以及数据中噪声量的影响。在直径为28 mm的氧化铝植入物中比较了三组直径公差。作者的假设是,随着测试持续时间的增加,磨损数据将得到显着改善。平均磨损率随测试持续时间变化不大,最大的变化仅使磨损估计值分别减少了30%和15%,减少了1000万次和1400万次。研究中最令人满意的改进是随着持续时间的增加,方差(噪声)的减少,在500万次循环时为±200%,在1400万次循环时为±55%。线性回归系数的质量在1000万次循环中提高了150%,在1400万次循环中提高了250%。总体上,直径公差最高的陶瓷植入物的磨损最少(减少15%,但无统计学意义)。但是,考虑到氧化铝衬套的磨损率如此之低,由于直径公差引起的任何差异在典型患者中不太可能具有临床意义。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号