This paper presents the results of an extensive experimental programme on typical cross-laminated timber (CLT) screwed connections conducted at CNR-IVALSA research institute. In-plane monotonic and cyclic shear and withdrawal tests were performed on screwed wall-to-wall, floor-to-floor and wall-to-floor CLT connections. Mechanical properties such as strength, stiffness, energy dissipation, ductility ratio and impairment of strength were evaluated. The experimental results showed good performance of CLT screwed joints under cyclic loads when ductile behaviour was achieved. Brittle response occurred only in cases where requirements for end and edge distances were not satisfied. The experimental characteristic shear strength and mean slip modulus of the connections were compared with values obtained using analytical design equations. The Eurocode 5 (EC5) formulas overestimated the characteristic strength values in some cases, while the Uibel and Blass formulas specifically developed for CLT connections provided more accurate and conservative predictions. In cases where brittle failures were attained, the analytical values overestimated the experimental ones. This issue can be avoided when the requirements for minimum edge and end distances stated by EC5 are fulfilled. EC5 empirical formulas for the prediction of the screw connection slip modulus at serviceability limit state corresponded well with the experimental elastic values. The overstrength factor, which is of great importance in capacity-based design, was also evaluated, and a conservative value of 1.6 can be recommended for screwed CLT connections.
机译:本文介绍了在CNR-IVALSA研究所进行的有关典型交叉层压木材(CLT)螺纹连接的广泛实验程序的结果。在螺纹式墙对墙,地板对地板和墙对地板CLT连接上进行了平面单调和循环剪切和拉拔测试。评估了机械性能,例如强度,刚度,能量耗散,延展性比和强度降低。实验结果表明,当循环载荷达到一定的延性时,CLT螺纹接头在循环载荷下具有良好的性能。脆性响应仅在不满足末端和边缘距离要求的情况下发生。将连接的实验特性抗剪强度和平均滑动模量与使用解析设计方程式获得的值进行比较。在某些情况下,欧洲规范5(EC5)公式高估了特征强度值,而专门为CLT连接开发的Uibel和Blass公式提供了更准确和保守的预测。在发生脆性破坏的情况下,分析值会高估实验值。当满足EC5规定的最小边缘和末端距离的要求时,可以避免此问题。用于预测使用寿命极限状态下的螺纹连接滑模量的EC5经验公式与实验弹性值非常吻合。还评估了在基于容量的设计中非常重要的超强度因素,对于螺钉式CLT连接,建议采用保守值1.6。

著录项

  • 来源
    《Holz als Roh- und Werkstoff》 |2015年第2期|179-191|共13页
  • 作者单位

    Department of Architecture, Design and Urban Planning, University of Sassari, Palazzo del Pou Salit, Piazza Duomo 6, 07041 Alghero, Italy;

    Department of Architecture, Design and Urban Planning, University of Sassari, Palazzo del Pou Salit, Piazza Duomo 6, 07041 Alghero, Italy;

    CNR IVALSA Trees and Timber Institute, Via Biasi 75, 38010 San Michele all'Adige, Italy;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

  • 入库时间 2022-08-17 23:29:17

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号