摘要

A novel carbon-sensitized and nitrogen-doped TiO_2 (C/N-TiO_2) was synthesized by a facile sol-gel method using titanium butoxide as both titanium precursor and carbon source, and nitric acid as nitrogen source. The calcination temperature had a great effect on the crystal phase structure, nitrogen incorporation into the TiO_2 lattice and content of carbonaceous species. The incorporated carbonaceous species could serve as photosensitizer, while the nitrogen doping could lead to the remarkable red shift of absorption edge of C/N-TiO_2. The C/N-TiO_2 calcinated at 300 ℃ (T300) exhibited the highest photocatalytic activity for sulfanilamide (SNM) degradation under irradiation of visible-light-emitting diode (vis-LED). The SNM photocatalytic degradation and mineralization were more efficient in acidic conditions due to the carbon photosensitizing effect. Insignificant inhibitory effects were observed in the presence of chloride, nitrate and sulfate, while bicarbonate, phosphate and silica could "Inhibit the SNM mineralization to different degrees. Acetate, ammonium and sulfate were released during SNM mineralization. T300 exhibited good photochemical stability and could be reused for 5 times with less than 10% decrease in the SNM removal efficiency. The acute toxicity of SNM solution could be reduced over prolonged photo-catalysis according to the Microtox assay.
机译:采用丁醇钛作为钛前驱体和碳源,硝酸为氮源,通过简便的溶胶-凝胶法合成了一种新型的碳敏氮掺杂的TiO_2(C / N-TiO_2)。煅烧温度对晶相结构,氮掺入TiO_2晶格和碳质含量有很大影响。掺入的碳质物质可作为光敏剂,而氮掺杂可导致C / N-TiO_2的吸收边缘发生明显的红移。在可见光发光二极管(vis-LED)的照射下,在300℃(T300)下煅烧的C / N-TiO_2表现出最高的磺酰胺(SNM)降解光催化活性。由于碳的光敏效应,在酸性条件下SNM光催化降解和矿化作用更为有效。在氯化物,硝酸盐和硫酸盐的存在下观察到微不足道的抑制作用,而碳酸氢盐,磷酸盐和二氧化硅可以“不同程度地抑制SNM矿化。乙酸,铵和硫酸盐在SNM矿化过程中被释放。T300具有良好的光化学稳定性并且可以重复使用5次,SNM去除效率降低不到10%,根据Microtox分析,长时间的光催化可以降低SNM溶液的急性毒性。

著录项

  • 来源
    《Water Research》 |2011年第16期|p.5015-5026|共12页
  • 作者单位

    School of Ciuil and Environmental Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798, Singapore Singapore Membrane Technology Centre, Nanyang Technological University, 50 Nanyang Auenue, Singapore 639798, Singapore;

    School of Ciuil and Environmental Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798, Singapore DHI-NTU Water and Environment Research Centre and Education Hub, Singapore 639798, Singapore;

    School of Ciuil and Environmental Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798, Singapore Singapore Membrane Technology Centre, Nanyang Technological University, 50 Nanyang Auenue, Singapore 639798, Singapore;

    School of Ciuil and Environmental Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798, Singapore Singapore Membrane Technology Centre, Nanyang Technological University, 50 Nanyang Auenue, Singapore 639798, Singapore;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Titanium dioxide; Carbon-sensitizing; Nitrogen-doping; Light-emitting diode; Sulfanilamide; Toxicity;

    机译:二氧化钛;碳敏化;氮掺杂发光二极管;磺胺;毒性;