Synroc immobilization of high level waste (HLW) bearing a high content of sodium

机译:含高钠含量的Synroc固定化高放废物(HLW)

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Synroc has been regarded as the second generation of high level waste (HLW) forms in the world. By isomorphous replacement most waste elements in HLW can be incorporated into the Synroc phases. The leach resistance and physical properties of Synroc are suitable for HLW immobilization. In general, sodium is not suitable for incorporation into Synroc. Two formulations, (Na_0.5Nd_0.5)TiO_3, perovskite type and Na_2(AlFe)_2Ti_6O_16, freudenbergite type were developed to immobilize higher content of Na_2O up to 5.7 and 5.0 wt /100, respectively. The present study greatly improved the sodium immobilization ability of Synroc.
机译:Synroc被视为世界上第二代高放废物(HLW)形式。通过同晶置换,可以将高放废物中的大多数废物元素纳入Synroc相。 Synroc的耐浸提性和物理性能适用于HLW固定。通常,钠不适合掺入Synroc。研制了钙钛矿型(Na_0.5Nd_0.5)TiO_3和铁矾土型Na_2(AlFe)_2Ti_6O_16两种配方,分别固定了更高的Na_2O含量,最高可达5.7和5.0 wt / 100。本研究大大提高了Synroc的钠固定能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号