The austenitizing treatment (1123-1223K, 1-2 hr) of austempered ductile irons (ADIs) was optimized by the correlation of results from thermal analysis and mechanical properties of ultimate tensile strength (UTS) and impact energy. Experimental results illustrated that a great UTS and optimum toughness were both in relation with great amounts of Q_sr and Q_se, and fast rate in heat evolution ( Q_sr/t_sr) during recalescence of austenite decom- position, where Q_sr and Q_se are heat evolved for the time period of recalescence and of terminating heat evolution, respectively. The optimized austenitizing treatment for austempered ductile irons developing their superior UTS was at 1173K for 1.5-1.75 hr and that, for performing optimum impact energy, was at l123K for 1.75-2.0 hours.
机译:奥氏体球墨铸铁(ADIs)的奥氏体化处理(1123-1223K,1-2 hr)通过热分析结果与极限拉伸强度(UTS)和冲击能量的机械性能的相关性进行了优化。实验结果表明,大量的UTS和最佳的韧性都与大量的Q_sr和Q_se以及奥氏体分解重新形成过程中的热放出速度快(Q_sr / t_sr)有关,其中Q_sr和Q_se产生热量。重新活化的时间段和终止放热的时间段。最佳奥氏体球墨铸铁的最佳奥氏体化处理是在1173K下进行1.5-1.75小时,而对于执行最佳冲击能,则在1123K下进行1.75-2.0小时。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号