AA6061-T4 composites containing SiC and B4C particles were fabricated by friction stir processing (FSP) with an SKD11 tool. The microstructures and mechanical properties of the composites were investigated with various test methods. With the inclusion of ceramic particles, refined grains in the stir zone (SZ) were observed using a scanning electron microscope (SEM) and tunneling electron microscope (TEM). Because the ceramic particles facilitated grain refinement in the SZ via the pinning effect, the SZ with the particles had a much smaller grain size than the SZ without the particles. Vickers hardness test, tensile test and Charpy impact test were conducted to evaluate the mechanical properties. Mechanical properties of the SZ with the ceramic particles were improved relative to those of the SZ without the particles. Vickers hardness (from 50 to 90 HV), tensile strength (from 117 to 253 MPa) and Charpy impact absorbed energy (from 4.2 to 5.6 J) of the SZ increased with the addition of ceramic particles.
机译:使用SKD11工具通过搅拌摩擦加工(FSP)制备了包含SiC和B4C颗粒的AA6061-T4复合材料。用各种测试方法研究了复合材料的微观结构和力学性能。在包含陶瓷颗粒的情况下,使用扫描电子显微镜(SEM)和隧道电子显微镜(TEM)观察到搅拌区(SZ)中的细晶粒。因为陶瓷颗粒通过钉扎效应促进了SZ中的晶粒细化,所以具有颗粒的SZ具有比没有颗粒的SZ小得多的晶粒尺寸。进行了维氏硬度试验,拉伸试验和夏比冲击试验以评估机械性能。与没有颗粒的SZ相比,具有陶瓷颗粒的SZ的机械性能得到改善。随着陶瓷颗粒的添加,SZ的维氏硬度(从50到90 HV),拉伸强度(从117到253 MPa)和夏比冲击吸收能量(从4.2到5.6 J)增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号