Carbonaceous fluorescent nanoparticles (CFNs) with broad particle distribution were synthesized by thermal-treatment using carbonation of silk cocoon as raw materials. The experimental results showed tunable emission wavelength of the nanoparticles. The quantum yield of the CFNs was calculated to be 23%. A CFNs/PVA hybrid thin film was prepared from a blend of the CFNs with polyvinyl alcohol (PVA) showing interesting green afterglow which could be observed by naked eyes. The afterglow spectrum revealed that the CFNs/PVA thin film had a broad afterglow emission peak located at 520 nm. The afterglow intensity decay curve of the film showed visually recognizable period longer than 140 s. The PVA-PVA hydrogen bonding in the PVA matrix may play a key role for the afterglow.
机译:以蚕茧的碳化为原料,通过热处理合成了粒径分布较宽的碳纳米管。实验结果表明纳米粒子的发射波长可调。 CFN的量子产率经计算为23%。由CFN与聚乙烯醇(PVA)的混合物制备CFN / PVA杂化薄膜,可以通过肉眼观察到这种绿色余辉。余辉光谱表明,CFNs / PVA薄膜在520 nm处具有较宽的余辉发射峰。薄膜的余辉强度衰减曲线显示出视觉上可识别的时间长于140 s。 PVA基质中的PVA-PVA氢键可能对余辉起关键作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号