Introducing a new specimen shape to assess the fatigue performance of asphalt mastic by dynamic shear rheometer testing

机译:引入新的试样形状以通过动态剪切流变仪测试来评估沥​​青胶泥的疲劳性能

获取原文
获取原文并翻译 | 示例
       

摘要

46.1-46.11%Early failure of asphalt pavements is a common issue all around the world. Damages are caused by various reasons like insufficient binder or aggregate quality, an inadequate mix design or improper handling in the production/construction process. The effects of binder, aggregates and mix design have been widely studied and state-of-the-art testing methods are available for both, hot-mix asphalt (HMA) and for each component. An important part in HMA belongs to the asphalt mastic, where no standardized method is available to allow a quality control. Asphalt mastic is the mix of bitumen with aggregates smaller than 63 (125) mu m and covers the coarse aggregates as the actual binding component in the mix. This research aims at developing a testing method for asphalt mastic based on fatigue tests. The dynamic shear rheometer (DSR) was found as a suitable device for this purpose. The DSR fatigue test consists of the 8 mm parallel-plate geometry widely used for binder performance grading with a sample height of 3 mm. Instead of a cylindrical specimen shape, a hyperboloid of one sheet is applied. This shape predetermines the point of failure and prevents adhesion/interface failures between the mastic specimen and the upper or lower DSR stainless steel plate. The specimens are prepared directly in the DSR employing a silicone mould to ensure an exact specimen shape. This test can be applied to all DSR devices without costly changes or additional equipment as long as sufficient cooling capacity and torque can be provided from the DSR. This fatigue test makes it possible to assess the fatigue performance of binders and mastic samples.
机译:46.1-46.11%沥青路面的早期破坏是世界各地的常见问题。损坏是由各种原因引起的,例如粘合剂或骨料质量不足,混合设计不足或生产/施工过程中的处理不当。粘合剂,集料和混合料设计的影响已得到广泛研究,并且对于热混合沥青(HMA)和每种组分都可以使用最新的测试方法。 HMA的重要组成部分是沥青胶泥,目前尚无标准化方法可进行质量控制。沥青胶泥是沥青的骨料,其骨料小于63(125)μm,并覆盖了作为骨料中实际粘结成分的粗骨料。这项研究旨在开发一种基于疲劳测试的沥青胶泥的测试方法。发现动态剪切流变仪(DSR)是用于此目的的合适设备。 DSR疲劳测试由8毫米平行板几何组成,广泛用于粘合剂性能分级,样品高度为3毫米。代替圆柱样品形状,使用一张双曲面。这种形状可确定破坏点,并防止乳香试样与DSR上下不锈钢板之间的粘附/界面破坏。使用硅树脂模具直接在DSR中制备样品,以确保精确的样品形状。只要DSR能够提供足够的冷却能力和扭矩,该测试就可以应用于所有DSR设备,而无需进行昂贵的更改或额外的设备。该疲劳测试可以评估粘合剂和乳香样品的疲劳性能。

著录项

  • 来源
    《Materials and structures》 |2018年第2期|136-146|共11页
  • 作者单位

    Vienna Univ Technol, Inst Transportat, Gusshausstr 28-E230-3, A-1040 Vienna, Austria;

    Vienna Univ Technol, Inst Transportat, Gusshausstr 28-E230-3, A-1040 Vienna, Austria;

    Vienna Univ Technol, Inst Transportat, Gusshausstr 28-E230-3, A-1040 Vienna, Austria;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Mastic; Filler; Fines; Fatigue; DSR;

    机译:Mastic;Filler;Fines;Fatigue;DSR;
  • 入库时间 2022-08-18 00:16:38

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号