This paper analyzes the configurations of the binding phases at different temperatures for 95W-5(Ni/Fe/Co) alloys by TEM, the precipitates of 95W-5(Ni/Fe/Co) alloys distribute dispersively at 300-500 deg C. So, it can make up for the fall of strength caused by the rise of temperature. Deformed at 600 deg C, the plasticity of the binding phases falls when the precipitates grow into stripes and distribute layer upon layer. Furthermore, owing to the discordance of the expansion coefficients of the two phases, internal stress forms, which reduces the integration strength at the boundary. The abnormity of plasticity change has close connection with temperature and precipitation.
机译:本文通过TEM分析了95W-5(Ni / Fe / Co)合金在不同温度下的键合相构型,其中95W-5(Ni / Fe / Co)合金的析出物在300-500℃分散分布。因此,它可以弥补由于温度上升而引起的强度下降。在600摄氏度变形时,当沉淀物长成条纹并逐层分布时,结合相的可塑性下降。此外,由于两相的膨胀系数不一致,形成了内部应力,这降低了边界处的积分强度。塑性变化的异常与温度和降水密切相关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号