Adhesive bonding of high-strength steel using epoxy (EP) and polyurethane (PU) adhesives was investigated. The steel surfaces were activated with dry ice blasting (DIB), and Self-Indicating Pretreatment (SIP)* coating was applied to improve the adhesion. Scanning electron microscopy (SEM), energy dispersive X-ray (EDX) analyses, and roughness measurements were carried out in addition to adhesive strength measurements. Our investigations indicate that adhesive strength improvement depends strongly on surface pretreatment, adhesive, and steel type. DIB improves the adhesion markedly. The combination of DIB plus SIP coating and EP adhesive increases the adhesive strength. The combination of DIB plus SIP coating and PU adhesive decreases the strength significantly. The increase in adhesive strength after DIB is due to the removal of contamination and lubricant layers. A further increase in adhesive strength after DIBÂ +Â SIP coating by EP adhesive is due to the use of SIP coating, which acts as a coupling agent between the adhesive and the steel surfaces. The significant decrease in adhesive strength with PU adhesive after DIBÂ +Â SIP coating is due to the increased size and number of closed bubbles in the adhesive layer, which act as stress raisers. DIB causes no changes in either topographic structure or surface roughness. EDX analysis of the treated surfaces indicates a reduction in carbon content and an increase in iron concentration.View full textDownload full textKeywordsAdhesion, Dry ice blasting, EDX, EP, High-strength steel, PU adhesives, SEM, SIP*, Surface roughnessRelated var addthis_config = { ui_cobrand: "Taylor & Francis Online", services_compact: "citeulike,netvibes,twitter,technorati,delicious,linkedin,facebook,stumbleupon,digg,google,more", pubid: "ra-4dff56cd6bb1830b" }; Add to shortlist Link Permalink http://dx.doi.org/10.1080/10426910903536774
机译:研究了使用环氧树脂(EP)和聚氨酯(PU)粘合剂的高强度钢的粘合方法。用干冰喷射(DIB)活化钢表面,并应用自指示预处理(SIP)*涂层以提高附着力。除粘合强度测量外,还进行了扫描电子显微镜(SEM),能量色散X射线(EDX)分析和粗糙度测量。我们的研究表明,粘合强度的提高在很大程度上取决于表面预处理,粘合剂和钢的类型。 DIB显着改善了附着力。 DIB加SIP涂层和EP粘合剂的结合可提高粘合强度。 DIB加SIP涂层和PU粘合剂的组合会显着降低强度。 DIB后粘合强度的提高是由于去除了污染物和润滑剂层。通过EP粘合剂进行DIB + SIP涂层后,粘合强度的进一步提高是由于使用了SIP涂层,该SIP涂层充当了粘合剂和钢表面之间的偶联剂。 DIB + SIP涂层后,PU粘合剂的粘合强度显着降低是由于粘合剂层中封闭的气泡的大小和数量增加,这些气泡起着应力的作用。 DIB不会改变地形结构或表面粗糙度。经过处理的表面的EDX分析表明碳含量降低,铁浓度增加。 = {ui_cobrand:“泰勒和弗朗西斯在线”,servicescompact:“ citeulike,netvibes,twitter,technorati,delicious,linkedin,facebook,stumbleupon,digg,google,更多”,发布:“ ra-4dff56cd6bb1830b”};添加到候选列表链接永久链接http://dx.doi.org/10.1080/10426910903536774

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号