We synthesized the La2/3Ca1/3MnO3 thin films on LaAlO3 (100) single-crystal substrates by a newly invented precursor film sintering (PFS) method. Thermal gravimetric analysis and Fourier transformation infrared spectroscopy (FTIR) analysis show that polyacrylamide, citric acid, and nitrite ions are burned out at a temperature higher than 600 degrees C, and La(1-x)A(x)MnO(3) oxides (LCMO) thin films begin to form at the same temperature. XRD results show that the LCMO thin films formed by the PFS method have the same crystal structure as the epitaxially grown LCMO thin films prepared by the pulsed laser deposition method. The maximum value of magneto-resistance (MR), 85.4%, has been observed at 259 K, and it can reach 40% even at room temperature. Besides, the advantages of the PFS method include simple equipments, common chemical compounds and a variety of shapes of the prepared thin films. (c) 2006 Elsevier B.V. All rights reserved.
机译:我们通过新发明的前驱膜烧结(PFS)方法在LaAlO3(100)单晶衬底上合成了La2 / 3Ca1 / 3MnO3薄膜。热重分析和傅立叶变换红外光谱(FTIR)分析表明,聚丙烯酰胺,柠檬酸和亚硝酸根离子在高于600摄氏度的温度下燃烧掉,并且La(1-x)A(x)MnO(3)氧化物(LCMO)薄膜开始在相同温度下形成。 XRD结果表明,通过PFS法形成的LCMO薄膜具有与通过脉冲激光沉积法制备的外延生长的LCMO薄膜相同的晶体结构。在259 K下观察到的最大磁阻(MR)值为85.4%,即使在室温下也可以达到40%。此外,PFS方法的优点包括简单的设备,常见的化学化合物以及制备的薄膜的各种形状。 (c)2006 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号