首页> 外文期刊>Journal of Analytical & Applied Pyrolysis >Effect of acid catalysts on scrap tyre pyrolysis under fast heating conditions
【24h】

Effect of acid catalysts on scrap tyre pyrolysis under fast heating conditions

机译:酸催化剂对快速加热条件下废轮胎热解的影响

获取原文
获取原文并翻译 | 示例
       

摘要

A study has been carried out on the effect of acid catalysts prepared based on HZSM-5, HY and HBeta zeolites on the distribution of volatile products (gas, non-aromatic C_5-C_(10) fraction, aromatic C_(10)- and tar), in the pyrolysis of tyre material carried out in a fast heating microreactor. The results have been compared with those of thermal pyrolysis. The strategies of using the catalyst in situ and reforming the volatiles generated in thermal pyrolysis have also been compared. The use of a catalyst in situ lowers the pyrolysis temperature by 50 K (to 723 K) and produces a significant increase in the yield of gases and light aromatic C_(10~-), at the expense of a decrease in the yield of non-aromatic C_(10~-). The yield of tar increases only slightly. The shape selectivity of each zeolite has a significant effect and, consequently, HY zeolite leads to the formation of heavier structures that make up the tar and to aromatic C_(10~-), which is favoured by hydrogen transfer capacity. HZSM-5 is more efficient for the formation of gases, although it contributes only to decreasing the molecular weight of aromatic C_(10~-) fraction. HBeta zeolite catalyst has an intermediate behaviour. Reforming pyrolysis volatiles at 723 K using a HZSM-5 zeolite catalyst efficiently increases (from 2 to 20 wt%) the yield of gases, with a high yield of ethene and propene. The yields of BTX fraction are also very high (around 11.5 wt%).
机译:已对基于HZSM-5,HY和HBeta沸石制备的酸催化剂对挥发性产物(气体,非芳族C_5-C_(10)馏分,芳族C_(10)-和芳烃)的分布进行了研究。焦油),在快速加热的微型反应器中对轮胎材料进行热解。将结果与热裂解的结果进行了比较。还比较了就地使用催化剂和重整热解过程中产生的挥发物的策略。原位使用催化剂可将热解温度降低50 K(至723 K),并显着提高气体和轻质芳烃C_(10--)的收率,但会降低非芳烃的收率。 -芳香族C_(10〜-)。焦油的收率仅略有增加。每种沸石的形状选择性都有很大的影响,因此,HY沸石会导致形成较重的结构,从而形成焦油并形成芳香族C_(10〜-),这受氢转移能力的推动。尽管HZSM-5仅有助于降低芳族C_(10〜-)馏分的分子量,但HZSM-5对于形成气体更有效。 HBeta沸石催化剂具有中间行为。使用HZSM-5沸石催化剂在723 K下重整热解挥发物可有效提高气体的收率(从2至20 wt%),并具有较高的乙烯和丙烯收率。 BTX馏分的收率也很高(约11.5 wt%)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号