Catalytic aquathermolysis of Omani heavy oil was carried out with NiMo-oleate as an oil soluble viscosity reducing catalyst and glycerol as a hydrogen donor for the first time. The synthesized catalyst was characterized with Fourier Transform Infrared Spectroscopy(FTIR) and X-ray diffraction (XRD). The experiments were carried out in a Parr reactor under nitrogen atmosphere with varying reaction time (24-72 h), glycerol concentration (0-10 wt%), catalyst loading(0-1 wt%), amount of water (0-42 wt%) and the reaction temperature (200-304 degrees C). Maximum viscosity reduction of 69% (1490-490 cP at 70 degrees C) occurred at 277 degrees C reaction temperature and 30 h of reaction. Fourier transform infrared spectra (FT-IR) before and after catalytic aquathermolysis show an increase in the saturate bonds of alkyl groups and a decrease in unsaturated bonds of transalkene groups of the hydrocarbons indicative of hydrogenation activities of the catalyst and glycerol. In addition, gas chromatography (GC) analysis confirmed an increase in lower boiling point components after catalytic aquathermolysis, while asphaltene precipitation showed a decrease in asphaltene content. (C) 2016 Elsevier B.V. All rights reserved.
机译:阿曼重油的催化水热解反应首次使用油溶性降粘催化剂NiMo-油酸酯和甘油作为氢供体进行。利用傅里叶变换红外光谱(FTIR)和X射线衍射(XRD)对合成的催化剂进行了表征。实验在氮气环境下在Parr反应器中进行,反应时间(24-72 h),甘油浓度(0-10 wt%),催化剂负载量(0-1 wt%),水量(0-42)有所不同wt%)和反应温度(200-304摄氏度)。在277摄氏度的反应温度和30个小时的反应中,最大粘度降低了69%(70摄氏度时为1490-490 cP)。催化水热解之前和之后的傅立叶变换红外光谱(FT-IR)表明,烷基的饱和键增加,而烃的反式链烯基的不饱和键减少,这表明催化剂和甘油的加氢活性。此外,气相色谱(GC)分析证实催化水热分解后较低沸点组分的增加,而沥青质沉淀表明沥青质含量降低。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号