In this study, we propose a new method of synthesizing Ni-Cu-Zn ferrite powder using steel pickled liquor and electroplating waste solutions as starting materials. It was found that the Ni-Cu-Zn ferrite powder prepared by a hydrothermal process from the waste solutions shows the formation of cubic ferrite with a saturation magnetization (M_s) of 31.5 emu/g and an intrinsic coercive force (H_(ci)) of 19.3 Oe. Upon annealing at 750℃ for 2 h, the saturation magnetization increases to 52.6 emu/g and the intrinsic coercive force reaches 42.8 Oe. This useful method can promote the recycling of industrial waste solution and contribute to the preservation of the earth. Moreover, this method decreases the manufacturing cost in the treatment of the industrial waste solution for electroplating and steel industries.
机译:在这项研究中,我们提出了一种以钢酸洗液和电镀废液为起始原料合成Ni-Cu-Zn铁氧体粉末的新方法。通过废液的水热法制备的Ni-Cu-Zn铁氧体粉末发现形成了立方铁氧体,其饱和磁化强度(M_s)为31.5 emu / g,固有矫顽力(H_(ci)) 19.3大江在750℃退火2h后,饱和磁化强度增加到52.6emu / g,固有矫顽力达到42.8Oe。这种有用的方法可以促进工业废液的回收利用,并有助于保护地球。而且,该方法降低了用于电镀和钢铁工业的工业废液的处理的制造成本。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号