Effects of dwell-times in the isothermal fatigue (IF) and thermal-mechanical fatigue (TMF) behaviors of six advanced high temperature materials are investigated in this paper; two of which belonged to types SS 304L and SS 304 stainless steels, two tantalum alloys; T-111 and ASTAR 811C, pure nickel Ni 201 and a nickel based, single crystal superalloy PWA 1480. The SS 304 and 304L steels were found to be sensitive under tensile dwells, however, effect of dwell-times was found to saturate with the increase in strain range (inelastic or total) for all materials examined. At lower strain ranges the effects of dwell-times were found to produce lower lives than at higher strains as in the case of AISI SS 304 and two tantalum based alloys T-111 and ASTAR 811C. Trends in various normalized life curves were found to be near sigmoidal for ASTAR 811 C, in which a typical inflection point could be found at nearly 0.2% inelastic strain range. Effects of dwell-times were more deleterious below that strain range and above 0.2% inelastic strain range the effects of dwell-times were nearly the same. Mechanistic aspects under different test conditions were-summarized.
机译:研究了停留时间对六种先进高温材料的等温疲劳(IF)和热机械疲劳(TMF)行为的影响。其中两种属于SS 304L和SS 304不锈钢,两种是钽合金。 T-111和ASTAR 811C,纯镍Ni 201和镍基单晶高温合金PWA1480。发现SS 304和304L钢在拉伸停留时间内很敏感,但是,停留时间的影响随着温度的升高而饱和。增加了所有检查材料的应变范围(无弹性或总应变)。与AISI SS 304和两种钽基合金T-111和ASTAR 811C的情况相比,在较低的应变范围内,发现停留时间的影响比在较高的应变下具有更长的寿命。对于ASTAR 811 C,发现各种归一化寿命曲线的趋势接近S形,其中典型的拐点可在近0.2%的非弹性应变范围内找到。在该应变范围以下和在0.2%非弹性应变范围以下,保压时间的影响更为有害。总结了不同测试条件下的机械性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号