The interfacial phenomena between molten pig iron and ilmenite prereduced with carbon and hydrogen were investigated. The wettability of prereduced ilmenite discs by molten pig iron was evaluated through measuring contact angle by the sessile droplet method. The effects of melting temperature, prereduction temperature and reduction degree on contact angle were examined. Molten pig iron could not be wetted by ilmenite prereduced with carbon and hydrogen, and the contact angle increases with increasing prereduction temperature. The contact angles of ilmenite prereduced with hydrogen are higher than that of ilmenite prereduced with carbon at the same reduction degree. The permeation of molten pig iron into porous ilmenite was observed at the interface of specimens prereduced with carbon and enhanced at higher reduction temperature. On the other hand, in the case of ilmenite prereduced with hydrogen, the permeation was not observed. These results indicate clearly that the separation between molten pig iron and reduced ilmenite can be enhanced by hydrogen reduction process, even at lower temperature than that of carbon reduction process.
机译:研究了碳和氢预还原的熔融生铁与钛铁矿之间的界面现象。通过使用无滴法测量接触角来评估熔融生铁对预还原钛铁矿圆片的润湿性。研究了熔融温度,预还原温度和还原度对接触角的影响。碳和氢预还原的钛铁矿不能润湿生铁水,并且接触角随预还原温度的升高而增加。在相同还原度下,氢预还原的钛铁矿的接触角大于碳预还原的钛铁矿的接触角。在用碳预还原并在较高还原温度下增强的试样的界面处观察到熔融生铁渗透到多孔钛铁矿中。另一方面,在用氢预还原钛铁矿的情况下,未观察到渗透。这些结果清楚地表明,即使在比碳还原过程更低的温度下,通过氢还原过程也可以增强熔融生铁和还原钛铁矿之间的分离。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号