This paper presents an experimental study of hydrogen production by alkaline water electrolysis using Zinc alloys as materials for cathode. The aim of this study is to select the best alloy for producing hydrogen on testing the effect of some operating parameters. Experiments were conducted on a water electrolysis cell with two electrodes (anode/ cathode). Throughout these experiments, we have chosen to use NaOH solution with different concentrations as an electrolyte. Binary alloys: Zn95%Fe5%, Zn90%Fe10%, Zn85% Fe15%, Zn95%Cu5%, Zn90%Cu10%, Zn85%Cu15%, Zn95%Co5%, Zn90%Co10%, Zn95%Cr5% and Zn90%Cr10% (mass %) were prepared as electrodes for the cathode. The effect of electrode composition, the electrolyte concentration, the voltage and amperage applied on volume of hydrogen produced are experimentally investigated. The results showed that the performance of alkaline water electrolysis is significantly affected by these various factors. Indeed, this preliminary study revealed that cathodes elaborated by (Zn95%Cr5%) and (Zn90%Cr10%) (mass %) produce more hydrogen gas than other alloys, in a minimum durations over the range of operating parameters tested. (C) 2017 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
机译:本文介绍了使用锌合金作为阴极材料通过碱性水电解制氢的实验研究。这项研究的目的是在测试某些操作参数的影响时,选择用于生产氢气的最佳合金。在具有两个电极(阳极/阴极)的水电解槽上进行了实验。在这些实验中,我们选择使用不同浓度的NaOH溶液作为电解质。二元合金:Zn95%Fe5%,Zn90%Fe10%,Zn85%Fe15%,Zn95%Cu5%,Zn90%Cu10%,Zn85%Cu15%,Zn95%Co5%,Zn90%Co10%,Zn95%Cr5%和Zn90%制备Cr10%(质量%)作为阴极的电极。实验研究了电极组成,电解质浓度,施加的电压和安培数对产生的氢气量的影响。结果表明,碱性水电解的性能受到这些因素的显着影响。确实,这项初步研究表明,由(Zn95%Cr5%)和(Zn90%Cr10%)(质量%)精心制作的阴极在所测试的运行参数范围内的最短持续时间内产生的氢气比其他合金更多。 (C)2017氢能出版物有限公司。由Elsevier Ltd.出版。保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号