High-density alumina was produced by fast firing (5 min, temperatures ≤ 550℃. Most of densificacion occurred under nonisothermal conditions. High densification rates observed are related to a change in the internal structure of the compact. The formation of a dense outer alumina layer controlled the heat flux to the interior of the compact, and increased the amount of energy available for sintering. Sintering in fast firing occurred as a densification front moving from the outer surface toward the sample center. As long as the rare of heat transfer is enough to sustain its advance, no differential densification occurs.
机译:快速烧结(5分钟,温度≤550℃)生产高密度氧化铝。大部分致密化发生在非等温条件下,观察到的高致密化速率与压坯的内部结构变化有关,形成了致密的外部氧化铝层控制着热流向坯体内部,并增加了可用于烧结的能量,由于致密化前沿从外表面向样品中心移动,因此发生了快速烧结的烧结过程,只要传热很少。足以维持其前进,不会发生差异致密化。

著录项

  • 来源
    《International journal of applied ceramic technology》 |2011年第6期|p.1486-1495|共10页
  • 作者单位

    Group of Ceramic and Glass Materials (CERMAT), Department of Chemical Engineering (EQA) and Department of Mechanical Engineering (EMC), Federal University of Santa Catarina, 88040-900 Florianopolis, SC, Brazil;

    Group of Ceramic and Glass Materials (CERMAT), Department of Chemical Engineering (EQA) and Department of Mechanical Engineering (EMC), Federal University of Santa Catarina, 88040-900 Florianopolis, SC, Brazil;

    Institute of Advanced Ceramics, Hamburg University of Technology (TUHH), 21071 Hamburg, Germany;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

  • 入库时间 2022-08-17 13:42:07

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号