Recrystallization behavior of a two-way cold rolled 12Cr ODS steel

机译:双向冷轧12Cr ODS钢的再结晶行为

获取原文
获取原文并翻译 | 示例
           

摘要

Recrystallization behavior of a two-way cold rolled 12Cr ODS steel during annealing in the range of 1273-1473 K was systemically investigated by means of scanning electron microscopy, electron backscatter diffraction, transmission electron microscopy, and hardness testing. Results show that original grains with 110 axis were rotated to 111 axis parallel to normal direction after similar to 60% reduction in thickness. Recovery stage was obvious at 1273 K annealing taking about 100 min, but at higher temperatures it was shortly followed by recrystallization. similar to 84% recrystallization was observed after annealing at 1473 K for 60 min, indicating that the new cold rolling process decreases the recrystallization temperature in comparison with the asfabricated specimen completing recrystallization at 1673 K. In addition, the microtexture evolution was characterized as recrystallization proceeded. The intensity of {111} 110 and {111} 112 components decreased, while intensive {110} 001 component was obtained. Dependence of the stored energy on the orientation of deformed grains is presumed for the reduction of {111} 110 and {111} 112 components, and oriented growth is probably responsible for the enhancement of {110} 001 texture after recrystallization.
机译:通过扫描电子显微镜,电子反向散射衍射,透射电子显微镜和硬度测试,系统地研究了双向冷轧12Cr ODS钢在1273-1473 K范围内的退火过程中的再结晶行为。结果显示,在厚度减少60%之后,将<110>轴的原始晶粒旋转到平行于法线方向的<111>轴。在1273 K退火耗时约100分钟时,恢复阶段很明显,但是在较高的温度下,很快就发生了重结晶。在1473 K下退火60分钟后,观察到类似于84%的再结晶,这表明与在1673 K下完成再结晶的预制试样相比,新的冷轧工艺降低了再结晶温度。此外,随着再结晶的进行,微观组织的演变得以表征。 {111} <110>和{111} <112>组分的强度降低,而获得了强烈的{110} <001>组分。据推测,储能与变形晶粒取向的相关性导致{111} <110>和{111} <112>组分的减少,取向生长可能是导致{110} <001>织构增强的原因。重结晶。

著录项

  • 来源
    《Fusion Engineering and Design》 |2019年第6期|99-105|共7页
  • 作者单位

    Univ Tokyo, Sch Engn, Nucl Profess Sch, 2-22 Shirakata Shirane, Tokai, Ibaraki 3191188, Japan;

    Univ Tokyo, Sch Engn, Nucl Profess Sch, 2-22 Shirakata Shirane, Tokai, Ibaraki 3191188, Japan;

    Chinese Acad Sci, Inst Met Res, 72 Wenhua Rd, Shenyang 110016, Liaoning, Peoples R China;

    Univ Tokyo, Sch Engn, Nucl Profess Sch, 2-22 Shirakata Shirane, Tokai, Ibaraki 3191188, Japan;

    Tohoku Univ, Inst Mat Res, 2-1-1 Katahira, Sendai, Miyagi 9808577, Japan;

    Hiroshima Inst Technol, Dept Intelligent Mech Engn, Saeki Ku, 2-1-1 Miyake, Hiroshima 7315193, Japan;

    Univ Tokyo, Sch Engn, Nucl Profess Sch, 2-22 Shirakata Shirane, Tokai, Ibaraki 3191188, Japan;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Oxide dispersion strengthened steels; Two-way cold rolling; Recrystallization; Microstructure; Microtexture;

    机译:氧化物弥散强化钢;双向冷轧;再结晶;显微组织;显微组织;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号