The Ce_(1-x)Y_(x)O_(2-x/2)samples were synthesized with different doping amount by solid state reaction method. Phase structures of the samples were analyzed and characterized by XRD. The effects of different doping amount on infrared emissivity properties at 3-5μm wavebands were investigated systematically. It is found that the powder with doping molality of x=0.2 exhibits the lowest infrared emissivity value ca. 0.21 when the test temperature is 600 °C. The mechanism for the low infrared emissivity is explored thoroughly. The reduction of infrared emissivity with increasing temperature is ascribed to the enhancement of electrical conductivity. Our results suggest that Ce_(1-x)Y_(x)O_(2-x/2)powder with x=0.2 is a potential candidate for stealth material of aircraft engines.
机译:通过固相反应法合成了不同掺杂量的Ce_(1-x)Y_(x)O_(2-x / 2)样品。样品的相结构通过XRD分析和表征。系统地研究了不同掺杂量对3-5μm波段红外发射率特性的影响。发现掺杂摩尔浓度为x = 0.2的粉末表现出最低的红外发射率值ca。测试温度为600°C时为0.21。深入探讨了低红外发射率的机理。红外发射率随温度升高而降低归因于电导率的提高。我们的结果表明,x = 0.2的Ce_(1-x)Y_(x)O_(2-x / 2)粉末是飞机发动机隐形材料的潜在候选者。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号