This study investigates the removal of silica and alumina as impurities from hematite based low-grade iron ore containing 34.18 mass% iron, 31.10 mass% of silica and 7.65 mass% alumina. Wet high-intensity magnetic separation (WHIMS) and reverse flotation (RF) were investigated. In WHIMS process, 93.08% of iron was recovered with a grade of 53.22 mass% at an optimum magnetic density of 10,000 mT, and pulp density of 2% used the L-4 machine. In RF experiments, optimal results showed 95.95% of iron recovered with 51.64 mass% grade using 1 kg/t of 1% alkaline starch as iron depressant and 1:1 mixture ratio of 0.75 kg/t DAA and NaOL as silica and alumina collectors. The designed multi-stage process involving feeding the concentrate from WHIMS into RF process reduced silica to 2.02 mass%, alumina to 1.04 mass% whilst recovering 81.94% of the iron with 67.27 mass% grade. As a result of this research, a process to produce high quality iron concentrate from hematite based low-grade iron ore with high iron recovery rate was constructed.
机译:这项研究研究了从赤铁矿基低品位铁矿石中去除作为杂质的二氧化硅和氧化铝的方法,该铁矿石包含34.18质量%的铁,31.10质量%的二氧化硅和7.65质量%的氧化铝。研究了湿式高强度磁选(WHIMS)和反向浮选(RF)。在WHIMS工艺中,以10,000 mT的最佳磁密度回收了93.08%的铁,品位为53.22质量%,使用L-4机的纸浆密度为2%。在射频实验中,最佳结果表明,使用1 kg / t的1%碱性淀粉作为抑铁剂,以及1:1 kg的0.75 kg / t DAA和NaOL的混合比作为二氧化硅和氧化铝收集剂,回收率为51.64质量%的95.95%的铁。设计的多阶段工艺涉及将WHIMS精矿进料到RF工艺中,将二氧化硅减少到2.02质量%,将氧化铝减少到1.04质量%,同时回收了81.94%的铁和67.27质量%的铁。作为这项研究的结果,构建了一种从铁矿石回收率高的赤铁矿基低品位铁矿石生产高质量铁精矿的方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号