Thermodynamic properties of the liquid Ag-Bi-Cu-Sn lead-free solder alloys

机译:液态Ag-Bi-Cu-Sn无铅焊料合金的热力学性质

获取原文
           

摘要

The electromotive force measurement method was employed to determine the thermodynamic properties of liquid Ag-Bi-Cu-Sn alloys using solid electrolyte galvanic cells as shown below: Kanthal+Re, Ag-Bi-Cu-Sn, SnO2 | Yttria Stabilized Zirconia | air, Pt, Experiments were made within temperature interval: 950 - 1300K along four composition paths of constant ratios: XAg : XBi : XCu = 1, XAg : (XBi + XCu) = 3:2 for XBi = XCu, XBi : (XAg + XCu) = 3:2 for XAg = XCu and XCu : (XAg + XBi) = 3:2 for XAg = XBi and tin concentration changing from 0.1 to 0.9 mole fractions, every 0.1. Almost all the results were approximated by straight line equations: EMF vs T, and tin activities were then calculated in arbitrary temperature; measurement results were presented by graphs. Unusual activity plot for XBi : (XAg + XCu) = 3:2 composition path was most probably caused by miscibility gap detected earlier in Bi-Cu-Sn ternary liquid alloys.
机译:电动势测量方法用于确定使用固态电解质原电池的液态Ag-Bi-Cu-Sn合金的热力学性质,如下所示:Kanthal + Re,Ag-Bi-Cu-Sn,SnO2 |氧化钇稳定的氧化锆|空气,Pt,在四个恒定比率的组成路径上的温度区间:950-1300K内进行实验:XBi = XCu,XBi:(XAg:XAg:XBi:XCu = 1,XAg:(XBi + XCu)= 3:2 XAg = XCu和XCu时+(XCu)= 3:2:XAg = XBi时(XAg + XBi)= 3:2,锡浓度每0.1从0.1到0.9摩尔分数变化。几乎所有结果均通过直线方程式近似:EMF与T,然后在任意温度下计算锡活度;测量结果由图表表示。 XBi:(XAg + XCu)= 3:2组成路径的异常活性图很可能是由Bi-Cu-Sn三元液态合金中较早检测到的混溶性间隙引起的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号