Study on In-Vitro Degradation of Bioabsorbable Polymers Poly (hydroxybutyrate-co-valerate) - (PHBV) and Poly (caprolactone) - (PCL)

机译:聚(羟基丁酸酯-共-戊酸酯)-(PHBV)和聚(己内酯)-(PCL)的可生物降解聚合物的体外降解研究

获取原文
           

摘要

The increasing use of bioabsorbable polymeric materials in medicine has stimulated researchers in the materials field to search for solutions for the replacement of metallic artifacts by bioabsorbable polymers. Therefore, this study describes the in vitro degradation of PHBV, PCL and the blends of these polymers, both of which are bioabsorbable polymers. The samples were prepared by extrusion followed by injection, and subjected submitted to in vitro degradation in phosphate buffered saline solution with pH 7.3 and kept at 37° C. Through the characterization of the variation of mass, molar mass, mechanical properties and morphology, the results indicated that the samples analyzed are more stable to hydrolytic degradation when compared to other bioabsorbable polymers. The materials indicate signs of degradation after 30 days, with a small reduction in the molar mass. After 180 days, the materials indicated a significant reduction of molar mass and reduction in the mechanical properties.
机译:生物可吸收聚合物材料在医学中的使用日益增加,刺激了材料领域的研究人员寻找可生物吸收聚合物替代金属伪影的解决方案。因此,这项研究描述了PHBV,PCL以及这些聚合物的共混物的体外降解,它们都是可生物吸收的聚合物。样品通过挤压制备,然后注射,然后在pH 7.3的磷酸盐缓冲盐溶液中进行体外降解,并保持在37°C下。通过表征质量,摩尔质量,力学性能和形态的变化,结果表明,与其他可生物吸收的聚合物相比,所分析的样品对水解降解更稳定。该材料在30天后显示出降解的迹象,摩尔质量略有下降。 180天后,材料表明摩尔质量显着降低,机械性能降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号