OBJECTIVE: The aim of this laboratory study is to evaluate the influence of the shape and the length limitation of superelastic nickel-titanium (NiTi) archwires on lower incisors inclination during alignment and leveling. METHODS: Metal teeth mounted on a typodont articulator device were used to simulate a malocclusion of the mandibular arch (-3.5 mm model discrepancy). Three different shapes (Standard, Accuform and Ideal) of superelastic NiTi archwires (Sentalloy, GAC, USA) were tested. Specimens were divided in two groups: Group I, with no limitation of the archwire length; and Group II, with distal limitation. Each group had thirty specimens divided into three subgroups differentiated by the archwire shape. All groups used round wires with diameters of 0.014-in, 0.016-in, 0.018-in and 0.020-in. The recording of all intervals was accomplished using standardized digital photographs with orthogonal norm in relation to median sagittal plane. The buccolingual inclination of the incisor was registered using photographs and software CorelDraw. RESULTS: The results were obtained using ANOVA and Tukey's test at a significant level of 5%. The inclination of the lower incisor increased in both groups and subgroups. The shape of the archwire had statistically significant influence only in Group I - Standard (11.76o), Ideal (5.88o) and Accuform (1.93o). Analyzing the influence of the length limitation, despite the mean incisor tipping in Group II (3.91o) had been smaller than Group I (6.52o), no statistically significant difference was found, except for Standard, 3.89o with limitation and 11.76o without limitation. The greatest incisor tipping occurred with the 0.014-in archwires.
机译:目的:本实验研究的目的是评估超弹性镍钛(NiTi)弓丝的形状和长度限制对对准和矫平过程中下门牙倾斜度的影响。方法:使用安装在台齿咬合器装置上的金属齿模拟下颌弓的咬合不正(-3.5 mm模型差异)。测试了三种不同形状(标准,准确和理想)的超弹性NiTi弓丝(Sentalloy,GAC,美国)。标本分为两组:第一组,没有弓丝长度的限制;第二组,没有弓丝长度的限制。第二组,远端受限。每组有三十个标本,按弓丝形状分为三个亚组。所有组均使用直径为0.014英寸,0.016英寸,0.018英寸和0.020英寸的圆线。所有间隔的记录都是使用标准化的数字照片完成的,该照片具有相对于中矢矢平面的正交标准。使用照片和软件CorelDraw记录了切牙的颊舌倾斜度。结果:使用方差分析和Tukey检验以5%的显着水平获得了结果。下切牙的倾斜度在组和亚组中均增加。弓丝的形状仅在I组中具有统计学上的显着影响-标准(11.76o),理想(5.88o)和Accuform(1.93o)。分析长度限制的影响,尽管第二组的平均门齿倾斜度(3.91o)小于第一组的平均门齿倾角(6.52o),但除标准,3.89o有限制和11.76o无外,均没有统计学上的显着差异。局限性。最大的门牙倾斜发生在0.014英寸弓丝中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号