The purpose of this study was to compare the compressive strength, diametral tensile strength and microhardnss of several selfadhesive resin cements (Rely-X U200, Clearfill SA Luting, G-CEM LinkAce, Maxcem Elite, PermaCem 2.0, and Zirconite) using different activation modes (self-cured, light-cured) and testing time (immediately, 24 h, thermocycling). Specimens were prepared for the compressive strength (? 4×6 mm) and diametral tensile strength and microhardness (? 6×3 mm) according to ISO standards. The strength after 24 h was higher than immediately after. In addition, G-CEM showed the highest values. In terms of the activation modes, Rely-X U200, PermaCem 2.0 had higher values in the light-curing than the self-curing. In conclusion, all cements demonstrated clinically available strength values and revealed differences in strength according to their composition, testing time and activation mode. Furthermore, correlation was found between the microhardness (degree of conversion) and mechanical strengths of the cements tested.
机译:这项研究的目的是比较使用不同活化方式的几种自粘树脂水泥(Rely-X U200,Clearfill SA Luting,G-CEM LinkAce,Maxcem Elite,PermaCem 2.0和Zirconite)的抗压强度,径向抗张强度和显微硬度。 (自固化,光固化)和测试时间(立即24小时,热循环)。根据ISO标准,制备抗压强度(≥4×6mm),径向拉伸强度和显微硬度(≥6×3mm)的样品。 24小时后的强度高于立即之后。另外,G-CEM显示出最高值。就激活模式而言,Rely-X U200,PermaCem 2.0在光固化中的值高于自固化。总之,所有水泥均表现出临床上可用的强度值,并根据其成分,测试时间和活化方式显示出强度差异。此外,在测试的水泥的显微硬度(转化度)和机械强度之间发现相关性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号