FTIR Spectral Evaluation of Polyurethane Adhesive Bonds in Perspex Canopies of Aircraft

机译:飞机有机玻璃机盖中聚氨酯胶粘剂的FTIR光谱评估

获取原文
获取外文期刊封面目录资料

摘要

Failure of capron glue (polyurethane) adhesive joint between nylon strips and perspex canopy of aircraft has been studied by Fourier transform infrared spectral analysis. It is concluded that the brittle failure of the joint is due to time-dependent crosslinking of residual isocyanate group with residual hydroxyl or the amino groups produced as a results of reaction of absorbed moisture with the isocyanate moiety: A service life of eight years has been estimated for the glue joint.
机译:通过傅里叶变换红外光谱分析,研究了尼龙条与飞机有机玻璃机盖之间的卡普龙胶(聚氨酯)胶接失效。结论是,接头的脆性破坏是由于残留的异氰酸酯基与残留的羟基或氨基的时间依赖性交联所致,该残留的羟基是由于吸收的水分与异氰酸酯部分反应而产生的:使用寿命为八年估计为胶接。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号