Iodine-doped TiO2was prepared by thermal hydrolysis of aqueous solutions of the titanium peroxo-complex, which includes no organic solvents or organometallic compounds. The synthesized samples were characterized by X-ray diffraction (XRD), Raman spectroscopy (RS), infrared spectroscopy (IR), specific surface area (BET), and porosity determination (BJH). The morphology and particle size was determined by high-resolution transmission electron microscopy (HRTEM) and selected area electron diffraction (SAED). All prepared samples have a red-shifted band-gap transition, well crystalline anatase structure, and porous particles with a 100–200 m2 g−1specific surface area. The photocatalytic activity of iodine-doped titania samples was determined by decomposition of Orange II dye during irradiation at 365 nm and 400 nm. Iodine doping promotes the titania photocatalytic activity very efficiently under visible light irradiation. The titania sample with 0.32 wt.% I has the highest catalytic activity during the photocatalyzed degradation of Orange II dye in an aqueous suspension in the UV and visible regions.
机译:碘掺杂的TiO2是通过将过氧钛络合物的水溶液进行热水解而制得的,该络合物不含有机溶剂或有机金属化合物。合成的样品通过X射线衍射(XRD),拉曼光谱(RS),红外光谱(IR),比表面积(BET)和孔隙率测定(BJH)进行表征。通过高分辨率透射电子显微镜(HRTEM)和选择区域电子衍射(SAED)确定形态和粒度。所有制备的样品均具有红移带隙跃迁,良好的锐钛矿结构和比表面积为100–200 m2 g-1的多孔颗粒。掺杂碘的二氧化钛样品的光催化活性通过在365nm和400nm的辐照过程中Orange II染料的分解来确定。碘掺杂在可见光照射下非常有效地促进了二氧化钛的光催化活性。在紫外和可见光区域的水悬浮液中,在光催化降解Orange II染料过程中,具有0.32%wt。%I的二氧化钛样品具有最高的催化活性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号