Chemical bath deposition was improved by using glycerol, a very conventional surfactant, to control cadmium sulfide CdS in various sizes and structures, under ultrasonic irradiation conditions. Consequently, an effective route to prepare CdS thin film that consists of either CdS fibrils with an average diameter of 52 nm or monodispersed CdS grains 35 to 80 nm in size is proposed. X-ray diffraction (XRD) studies revealed that, in the crystallographic properties of the obtained CdS films, CdS may exist in two crystalline modifications—a hexagonal and a cubic phase—that are characterized by several diffraction peaks positioned at 2θ≈23.4°, 27.1° and 47.8°. Beside this, UV-Vis studies also revealed the positive effect of glycerol at grain boundaries, leading to detrimental reduction of the band bending towards the absorber surface and increasing the population of optical absorptions.
机译:通过在超声波辐射条件下使用甘油(一种非常传统的表面活性剂)来控制各种尺寸和结构的硫化镉CdS,可以改善化学浴的沉积。因此,提出了一种制备由平均直径为52nm的CdS原纤维或尺寸为35-80nm的单分散CdS晶粒组成的CdS薄膜的有效途径。 X射线衍射(XRD)研究表明,在获得的CdS膜的晶体学性质中,CdS可能以两种晶型(六方相和立方相)存在,其特征是位于2θ≈23.4°处的几个衍射峰, 27.1°和47.8°。除此之外,UV-Vis研究还揭示了甘油在晶界处的积极作用,导致朝向吸收体表面弯曲的能带有害减少,并增加了光吸收的范围。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号