In this study the electric arc furnace slag was used as coarse natural aggregate substitute in concrete paving blocks production. The concrete mixture was defined by using weight proportions in the ratio of 1:2:3:0.51 (cement:sand:coarse aggregate:water) in order to obtain a compressive strength of 35 MPa. Four groups of concrete were prepared: a reference recipe and three others with the slag replacing the natural aggregate in the proportions of 25%, 50% and 75%. The compressive strength was not influenced by the slag content; however, it was influenced by the curing age, as the sample with 75% of slag addition had its compressive strength increased by 13.5% from 7 to 56 days. Water absorption presented a slightly reduction with slag addition. The results of compressive strength and water absorption met the Brazilian technical requirements, making the paving blocks suitable for use in light vehicle traffic. The results obtained in this study highlight the influence of the production process in the final quality of the steel slag, and the need of stablishing technical and environmental requirements to guide and promote the safe use of electric arc furnace slag in concrete.
机译:在这项研究中,电弧炉炉渣被用作混凝土铺路砖生产中的天然粗骨料替代品。通过使用重量比为1:2:3:0.51(水泥:砂子:粗骨料:水)的比例来定义混凝土混合物,以获得35 MPa的抗压强度。准备了四组混凝土:参考配方和三组混凝土,其中矿渣以25%,50%和75%的比例代替了天然骨料。抗压强度不受炉渣含量的影响;但是,它受固化时间的影响,因为添加了75%的炉渣的样品的抗压强度从7天到56天增加了13.5%。吸水率随加入矿渣而略有降低。抗压强度和吸水率的结果满足了巴西的技术要求,这使铺路砖适用于轻型车辆通行。这项研究获得的结果突出了生产过程对钢渣最终质量的影响,以及需要确立技术和环境要求以指导和促进电弧炉渣在混凝土中的安全使用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号