Effect of blend ratio and coagulation bath temperature on the morphology, tensile strength and performance of cellulose acetate/poly(butylene succinate) membranes

机译:共混比和凝固浴温度对醋酸纤维素/聚丁二酸丁二醇酯膜的形貌,拉伸强度和性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

In the present study, blend membranes of cellulose acetate (CA)/poly(butylene succinate) (PBS) were prepared. The membrane morphology, tensile strength and performance in bread wastewater treatment were evaluated in terms of the membrane preparation conditions. According to the results, presence of PBS varied the membrane structure by reducing the extension of macro pores in the membrane sublayer. CA could effectively improve tensile strength of the membranes. Reducing coagulation bath temperature resulted in obtaining the membranes with denser structure and also higher tensile strength. Considering differences in surface and cross-sectional structures, the membranes with PBS content of 85 and 100% were found to have the highest separation ability, whereas the highest flux belonged to the membrane with 50% PBS.
机译:在本研究中,制备了醋酸纤维素(CA)/聚丁二酸丁二酯(PBS)的共混膜。根据制膜条件,评价了面包废水处理中的膜形态,拉伸强度和性能。根据结果​​,PBS的存在通过减少膜亚层中大孔的延伸来改变膜结构。 CA可以有效地提高膜的拉伸强度。降低凝固浴温度导致获得具有更致密结构和更高拉伸强度的膜。考虑到表面和横截面结构的差异,发现PBS含量分别为85%和100%的膜具有最高的分离能力,而通量最高的膜属于PBS含量为50%的膜。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号