Can 1% chlorhexidine diacetate and ethanol stabilize resin-dentin bonds?

机译:1%的氯己定双乙酸盐和乙醇能否稳定树脂-牙本质键?

获取原文
获取原文并翻译 | 示例
       

摘要

Objectives. To examine the effects of the combined use of chlorhexidine and ethanol on the durability of resin-dentin bonds. Methods. Forty-eight flat dentin surfaces were etched (32% phosphoric acid), rinsed (15 s) and kept wet until bonding procedures. Dentin surfaces were blot-dried with absorbent paper and re-wetted with water (water, control), 1% chlorhexidine diacetate in water (CHD/water), 100% ethanol (ethanol), or 1% chlorhexidine diacetate in ethanol (CHD/ethanol) solutions for 30 s. They were then bonded with All Bond 3 (AB3, Bisco) or Excite (EX, Ivoclar-Vivadent) using a smooth, continuous rubbing application (10 s), followed by 15 s gentle air stream to evaporate solvents. The adhesives were light-cured (20 s) and resin composite build-ups constructed for the microtensile method. Bonded beams were obtained and tested after 24-h, 6-months and 15-months of water storage at 37 ℃. Storage water was changed every month. Effects of treatment and testing periods were analyzed (ANOVA, Holm-Sidak, p < 0.05) for each adhesive. Results. There were no interactions between factors for both etch-and-rinse adhesives. AB3 was significantly affected only by storage (p=0.003). Excite was significantly affected only by treatments (p = 0.048). AB3 treated either with ethanol or CHD/ethanol resulted in reduced bond strengths after 15 months. The use of CHD/ethanol resulted in higher bond strengths values for Excite. Conclusions. Combined use of ethanol/1% chlorhexidine diacetate did not stabilize bond strengths after 15 months.
机译:目标。研究洗必泰和乙醇的组合使用对树脂-牙本质键耐久性的影响。方法。刻蚀四十八个平坦的牙本质表面(32%磷酸),冲洗(15 s)并保持湿润,直到粘合程序为止。牙本质表面用吸水纸吸干,然后用水(水,对照),1%的双乙酸洗必太水溶液(CHD /水),100%的乙醇(乙醇)或1%的双氯洗必太乙醇(CHD /乙醇溶液)30 s。然后使用光滑,连续的摩擦(10 s),然后用15 s温和的气流蒸发溶剂,将它们与All Bond 3(AB3,Bisco)或Excite(EX,Ivoclar-Vivadent)粘合。将粘合剂光固化(20 s),并为微拉伸方法构建树脂复合材料。在37℃贮水24小时,6个月和15个月后,获得并测试了粘结梁。每月更换储水量。分析每种胶粘剂的处理和测试时间的影响(ANOVA,Holm-Sidak,p <0.05)。结果。蚀刻和冲洗粘合剂的因素之间没有相互作用。 AB3仅受存储显着影响(p = 0.003)。兴奋仅受治疗显着影响(p = 0.048)。 15个月后,用乙醇或CHD /乙醇处理过的AB3导致粘结强度降低。 CHD /乙醇的使用导致Excite的粘结强度值更高。结论。 15个月后,乙醇/ 1%氯己定双乙酸盐的联合使用不能稳定结合强度。

著录项

  • 来源
    《Dental materials》 |2014年第7期|735-741|共7页
  • 作者单位

    University of British Columbia, Faculty of Dentistry, Department of Oral Biological and Medical Sciences, Division of Biomaterials, Vancouver, BC, Canada,University of Sao Paulo, School of Dentistry, Department of Dental Biomaterials and Biochemistry, Sao Paulo, SP, Brazil;

    University of Sao Paulo, School of Dentistry, Department of Dental Biomaterials and Biochemistry, Sao Paulo, SP, Brazil;

    University of Illinois at Chicago, College of Dentistry, Department of Restorative Dentistry, Chicago, IL, USA;

    University of Ponta Grossa, School of Dentistry, Department of Restorative Dentistry, Ponta Grossa, PR, Brazil;

    University of Ponta Grossa, School of Dentistry, Department of Restorative Dentistry, Ponta Grossa, PR, Brazil;

    Georgia Regents University, College of Dental Medicine, Department of Oral Biology and Maxillofacial Pathology, Augusta, GA, USA;

    University of British Columbia, Faculty of Dentistry, Department of Oral Biological and Medical Sciences, Division of Biomaterials, Vancouver, BC, Canada;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《化学文摘》(CA);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Ethanol-wet bonding; Chlorhexidine; Dentin; Bonding; Stability;

    机译:乙醇湿粘结;洗必太;牙本质粘接;稳定性;