Ae Response Of Type 304 Stainless Steel During Stress Corrosion Crack Propagation

机译:304型不锈钢在应力腐蚀裂纹扩展过程中的Ae响应

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

Acoustic emission (AE) signals generated by transgranular stress corrosion cracking (TGSCC) and inter-granular stress corrosion cracking (IGSCC) have been compared by means of slow strain rate tensile tests (SSRT) performed using both solubilised and sensitised type AIS1 304 stainless steel in a 1 M NaCl + 1M HCl solution. Results show that the AE activity during the propagation of TGSCC is much higher than the AE activity during the IGSCC propagation. However, no significant difference was found between the mean amplitude and rise-time of the AE signals registered during the propagation of TGSCC and those measured for IGSCC propagation.
机译:通过使用增溶型和增感型AIS1 304不锈钢进行的慢应变速率拉伸试验(SSRT),比较了跨晶应力腐蚀开裂(TGSCC)和晶间应力腐蚀开裂(IGSCC)产生的声发射(AE)信号。在1 M NaCl + 1M HCl溶液中。结果表明,TGSCC传播过程中的AE活性远高于IGSCC传播过程中的AE活性。但是,在TGSCC传播期间记录的AE信号与为IGSCC传播测量的AE信号的平均幅度和上升时间之间没有发现显着差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号