Quantitative assessment of local misorientations and pitting corrosion behaviour of pearlitic steel using electron backscattered diffraction and microcapillary techniques

机译:使用电子背散射衍射和微毛细管技术定量评估珠光体钢的局部取向和点蚀行为

获取原文
获取原文并翻译 | 示例

摘要

The influence of the grain tolerance angle (GTA) on the microstructural parameters of pearlitic steel is investigated using electron backscattered diffraction. The corrosion behavior of this alloy is then evaluated from local polarisation curves (electrochemical microcell technique) and potentiostatic pulse testing. These results are analyzed according to the specimen microstructure (grain boundaries and grain orientation spread, GOS). It is shown that there is a critical value of the GOS (around 10 degrees) leading to significant decrease of the pitting potential. The influence of the GTA value on the analysis of electrochemical results is also discussed. (C) 2015 Elsevier Ltd. All rights reserved.
机译:利用电子背散射衍射研究了晶粒公差角(GTA)对珠光体钢组织参数的影响。然后根据局部极化曲线(电化学微电池技术)和恒电位脉冲测试评估该合金的腐蚀行为。根据样品的微观结构(晶粒边界和晶粒取向扩展,GOS)分析这些结果。结果表明,GOS存在一个临界值(约10度),导致点蚀电位显着降低。还讨论了GTA值对电化学结果分析的影响。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号