A Mechanistic-Empirical (M-E) design based pavement quality or performance prediction methodology incorporating nondestructive test such as Ground Penetrating Radar (GPR) and Falling Weight Deflectometer (FWD) tests is demonstrated in this study. To facilitate, three pavement sites, namely, US285, US54, and I-40 in New Mexico are selected for nondestructive tests such as GPR and FWD. It is observed that the GPR predicted AC layer thickness is more consistent than base layer thickness. The FWD test was also conducted on the same locations, and like GPR, backcalculated layer moduli also shows varying level of inconsistency in different pavement sections. Based on the GPR and FWD tests, each of these three sites is divided into two major areas: one with the mean and the other with the minimum layer thicknesses and modulus. Layer thicknesses as well as moduli are incorporated to the AASHTOWare-ME software to determine load related distresses such as bottom-up crack and rut. Based on the amount of bottom-up cracks, the US54 pavement section is predicted to fail during 15th year of its service life, and the time of failure can be very early in the area with minimum layer thickness and modulus. Based on the rut prediction, pavement sections in US54 and I-40 is predicted to fail early. Finally, this methodology is recommended to implement to perform pavement quality assessment incorporating GPR and FWD tests in both project and network levels. (C) 2017 Elsevier Ltd. All rights reserved.
机译:在这项研究中,展示了一种基于机械-经验(M-E)设计的路面质量或性能预测方法,该方法结合了无损测试,例如探地雷达(GPR)和落锤挠度计(FWD)测试。为方便起见,在新墨西哥州选择了三个铺面现场,分别是US285,US54和I-40,以进行无损检测,例如GPR和FWD。可以看出,GPR预测的AC层厚度比基础层厚度更一致。 FWD测试也在相同的位置进行,并且像GPR一样,反算的层模量也显示出不同路面截面中不同程度的不一致性。根据GPR和FWD测试,这三个位置中的每个都分为两个主要区域:一个具有平均值,另一个具有最小的层厚度和模量。 AASHTOWare-ME软件结合了层厚度和模量,以确定与载荷有关的应力,例如自下而上的裂纹和车辙。根据自下而上的裂缝数量,预计US54路面在其使用寿命的15年内会发生故障,并且在层厚度和模量最小的区域中,破坏时间可能非常早。根据车辙预测,预计US54和I-40中的人行道路段将尽早失效。最后,建议采用这种方法来进行路面质量评估,并在项目和网络层面进行GPR和FWD测试。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号