The present study describes the synthesis of ZnMn2O4 nanoparticles with the spinel structure. These oxide nanoparticles are obtained from the decomposition of metal oxalate precursors synthesized by (a) the reverse micellar and (b) the coprecipitation methods. Our studies reveal that the shape, size and morphology of precursors and oxides vary significantly with the method of synthesis. The oxalate precursors prepared from the reverse micellar synthesis method were in the form of rods (micron size), whereas the coprecipitation method led to spherical nanoparticles of size, 40–50 nm. Decomposition of oxalate precursors at low temperature (∼ 450°C) yielded phase pure ZnMn2O4 nanoparticles. The size of the nanoparticles of ZnMn2O4 obtained from reverse micellar method is relatively much smaller (20–30 nm) as compared to those made by the co-precipitation (40–50 nm) method. Magnetic studies of nanocrystalline ZnMn2O4 confirm antiferro-magnetic ordering in the broad range of ∼ 150 K. The photocatalytic activity of ZnMn2O4 nanoparticles was evaluated using photo-oxidation of methyl orange dye under UV illumination and compared with nanocrystalline TiO2.
机译:本研究描述了具有尖晶石结构的ZnMn 2 O 4 纳米颗粒的合成。这些氧化物纳米颗粒是通过(a)反胶束和(b)共沉淀法合成的草酸金属前体的分解获得的。我们的研究表明,前体和氧化物的形状,大小和形态随合成方法的不同而有很大差异。用逆胶束合成法制得的草酸盐前体为棒状(微米级),而共沉淀法制得的球形纳米颗粒尺寸为40-50 nm。草酸盐前体在低温(约450°C)下分解产生相纯的ZnMn 2 O 4 纳米颗粒。通过逆胶束法获得的ZnMn 2 O 4 纳米粒子的尺寸与共沉淀法相比要小得多(20–30 nm)( 40–50 nm)方法。纳米ZnMn 2 O 4 的磁性研究证实了反铁磁有序在约150 K的宽范围内。ZnMn 2 O的光催化活性用甲基橙染料在紫外光下的光氧化作用评估了 4 纳米颗粒,并与纳米晶TiO 2 进行了比较。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号