This paper presents the results of the static tensile and fatigue life tests under rotating bending of round 1.4301 (AISI 304) steel samples. The fatigue tests were carried out on smooth and notched samples with three different rounding angles with a shape factor of 1.4, 2 and 2.6. A fatigue life was determined for samples with different shape factors subject to identical loads. The results showed that the scatter of fatigue test results decreases with an increase in shape factor. To evaluate the cracking properties (cracking mode and mechanism), microstructure and fractographic tests of the fractured samples were carried out.
机译:本文介绍了圆形1.4301(AISI 304)钢样品在旋转弯曲下的静态拉伸和疲劳寿命测试结果。在具有三个不同的圆角,形状系数分别为1.4、2和2.6的光滑且有缺口的样品上进行了疲劳测试。确定了具有相同载荷的具有不同形状因子的样品的疲劳寿命。结果表明,疲劳试验结果的散布随形状因子的增加而减小。为了评估开裂性能(开裂方式和机理),对断裂样品进行了显微组织和分形测试。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号