The internal defects and shape of cyclotrimethylenetrinitramine (RDX) crystal are critical parameters for the preparation of reduced sensitivity RDX (RS-RDX). In the current study, RDX was re-crystallized and spheroidized to form the high-quality RDX that was further characterized by purity, apparent density, size distribution, specific surface area, impact sensitivity, and shock sensitivity. The effects of re-crystallization solvent on the growth morphology of RDX crystal were investigated by both theoretical simulation and experiment test, and consistent results were obtained. The high-quality RDX exhibited a high purity (≥99.90%), high apparent density (≥1.811 g/cm3), spherical shape, and relatively low impact sensitivity (6%). Its specific surface area was reduced more than 30%. Compared with conventional RDXs, the high-quality RDX reduced the shock sensitivities of PBXN-109 and PBXW-115 by more than 30%, indicating that it was a RS-RDX. The reduced sensitivity and good processability of the high-quality RDX would be significant in improving the performances of RDX-based PBXs.
机译:环三亚甲基三硝胺(RDX)晶体的内部缺陷和形状是制备灵敏度降低的RDX(RS-RDX)的关键参数。在当前的研究中,RDX被重结晶和球化以形成高质量的RDX,其特征还在于纯度,表观密度,尺寸分布,比表面积,冲击敏感性和冲击敏感性。通过理论模拟和实验测试研究了重结晶溶剂对RDX晶体生长形态的影响,并获得了一致的结果。高质量的RDX具有高纯度(≥99.90%),高表观密度(≥1.811g / cm 3 ),球形和相对较低的冲击敏感度(6%)。其比表面积减少了30%以上。与传统的RDX相比,高质量的RDX将PBXN-109和PBXW-115的震动敏感性降低了30%以上,表明它是RS-RDX。高质量R​​DX的降低的灵敏度和良好的可加工性对于改善基于RDX的PBX的性能将具有重要意义。