Effect of Non-Vital Bleaching on the Durability of Resin–Dentin Bond with an Ethanol-Based Etch-And-Rinse Adhesive

机译:非重要漂白剂对基于乙醇的蚀刻和冲洗粘合剂的树脂-牙本质键耐久性的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

To evaluate the bleaching procedure and application of sodium ascorbate on dentin bond durability, the enamel surface of intact human third molars (n = 18) were removed, and the teeth were randomly divided into two groups for immediate and six-month bond strength evaluation. The specimens were further assigned into three subgroups according to treatment procedure, as follows: subgroup A, no bleaching (positive control) was performed prior to the etch-and-rinse bonding with single bond and subsequent build-up with Z250 composite; subgroup B, the samples were bleached with 20% carbamide peroxide 6 h/day for five consecutive days prior to bonding; and subgroup C, bleaching was performed as in subgroup B, after which 10% sodium ascorbate was applied on dentin surface for 10 min before the bonding procedures. A microtensile bond strength test was performed and the failure modes were evaluated under a stereomicroscope. The data were analyzed using two-way analysis of variance (ANOVA) and Tukey’s post-hoc tests with a level of significance of 0.05. Bleaching significantly decreased the immediate and six-month bond strength. The application of sodium ascorbate had no significant effect on the immediate and six-month bond strength of bleached specimens. We conclude that the bleaching procedure may decrease the durability of the resin–dentin bond of the tested etch-and-rinse adhesive.
机译:为了评估漂白程序和抗坏血酸钠对牙本质粘结耐久性的影响,去除了完整的人类第三磨牙(n = 18)的釉质表面,将牙齿随机分为两组,以进行即刻和六个月的粘结强度评估。根据处理程序,将样品进一步分为三个亚组:A亚组,在进行单键蚀刻和漂洗键合之前未进行漂白(阳性对照),随后使用Z250复合材料进行固结。在B组中,在粘结前连续5天用20%的过氧化脲漂白样品6小时/天。在C组和C组中,与B组一样进行漂白,然后在粘结步骤之前将10%抗坏血酸钠施加在牙本质表面上10分钟。进行了微拉伸粘合强度测试,并在立体显微镜下评估了破坏模式。使用双向方差分析(ANOVA)和Tukey事后检验对数据进行了分析,显着性水平为0.05。漂白显着降低了立即和六个月的粘合强度。抗坏血酸钠的使用对漂白样品的即时和六个月粘结强度没有显着影响。我们得出的结论是,漂白程序可能会降低经过测试的蚀刻和冲洗粘合剂的树脂-牙本质键的耐久性。