Analogous Anti-Ferroelectricity in Y2O3-Coated (Pb0.92Sr0.05La0.02)(Zr0.7Sn0.25Ti0.05)O3 Ceramics and Their Energy-Storage Performance

机译:Y2O3涂层(Pb0.92Sr0.05La0.02)(Zr0.7Sn0.25Ti0.05)O3陶瓷中的类似反铁电性及其储能性能

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Antiferroelectric analogous (Pb0.92Sr0.05La0.02)(Zr0.7Sn0.25Ti0.05)O3 (PSLZSnT) ceramics were prepared by the solid-state sintering method by introducing a Y2O3-coating via the self-combustion method. The synthesized Y2O3-doped PSLZSnT ceramics present pseudo-cubic structure and rather uniform microstructural morphology accompanied by relatively small grain size. Excellent energy-storage performance is obtained in the Y2O3-doped PSLZSnT ceramics, in which the value of the energy-storage density presents a linearly increasing trend within the electric field measurement range. Such excellent performance is considered as relating to the rather pure perovskite structure, high relative density accompanied by relatively small grain size, and the antiferroelectric-like polarization-electric field behavior.
机译:通过自烧结法引入Y 2 O 3涂层,通过固态烧结法制备了反铁电类似(Pb0.92Sr0.05La0.02)(Zr0.7Sn0.25Ti0.05)O3(PSLZSnT)陶瓷。合成的Y2O3掺杂的PSLZSnT陶瓷具有伪立方结构,并且具有均匀的微观结构形态,同时具有相对较小的晶粒尺寸。掺Y2O3的PSLZSnT陶瓷具有出色的储能性能,其中储能密度的值在电场测量范围内呈线性增加趋势。这种优异的性能被认为与钙钛矿结构相当纯净,相对密度高,晶粒尺寸相对较小以及类反铁电极化电场行为有关。