提高把手喷涂产品成品率的研究

             

摘要

针对客户把手喷涂产品存在表面麻点缺陷,成品率仅为29.41%的问题,本文在生产实践的基础上,分析了产品出现缺陷的具体原因,并对产品质量的改进措施进行了研究.结果表明,产品的缺陷主要是由基材表面的颗粒、夹渣及纹路造成,通过采用喷砂、碱蚀、返喷和化学修复剂修复等措施,可将把手喷涂产品合格率稳定在90%以上.%urface pitting defects exist on the customer's hand spray products,lead to the yield of only 29.41%.In view of this problem,the specific reasons for the defects of the product were analyzed based on the productive practice,and the improvement measures of product quality were researched.The results showed that defect of the product was mainly caused by particles,slag and grain on the surface of the substrate.Product percent of pass could be stabilized over 90% through abrasive blasting,alkaline etching,second-spray and repair using chemical reparation agent.

著录项

  • 来源
    《电镀与精饰》 |2018年第5期|34-36|共3页
  • 作者单位

    湖南省计量检测研究院,湖南长沙410014;

    南南铝业股份有限公司,广西南宁530031;

    湖南省计量检测研究院,湖南长沙410014;

    南南铝业股份有限公司,广西南宁530031;

    湖南省计量检测研究院,湖南长沙410014;

    南南铝业股份有限公司,广西南宁530031;

    南南铝业股份有限公司,广西南宁530031;

    湖南省计量检测研究院,湖南长沙410014;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 印刷电路;
  • 关键词

    把手; 麻点; 喷砂; 碱蚀; 返喷; 修复;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号