In order to decrease the solubility of PbSO4 and enhance lead recovery from PbSO4 bearing wastes, CO was employed as a reductant to transform PbSO4 into Pb S. Reaction system was established and reductive thermodynamics of PbSO4 was calculated by software HSC 5.0. The effects of gas concentration, reaction temperature, time and mass of sample on reduction of PbSO4 were examined by thermogravimetry(TG) and XRD. Roasting tests further verify the conclusions of thermodynamic and TG analyses. The results show that increasing temperature in the reasonable range and CO content are favorable for the formation of Pb S. The reduction process is controlled by chemical reaction and calculation value of the activation energy is 47.88 k J/mol.