T his paper introduces the process of using the electric furnace slag as raw material , and using the centrifugal equipment to make the fiber . The effection of different slags to the properties on swing fibers for making paper are compared . The results show that slag temperature has reached 1 600℃ , CaO was added to 5% can be made of inorganic mineral fiber . In the process of papermaking add 45% inorganic min‐eral fiber to box board paper with national B standards .%介绍了以电炉炉渣为原料,采用离心设备甩制纤维的工艺过程,再对比不同炉渣对甩制纤维性能的影响和纤维对造纸性能的影响。结果表明:炉渣温度达到1600℃、CaO添加量5%可以制得无机矿物纤维,在造纸过程中添加45%无机矿物纤维制得的箱板纸符合国家B类标准。