By analyzing the ore elements contained in calcined ginger nut, calcined Aga soil, and Europe hydraulic lime NHL5, and by comparing the mechanics of the three materials with concretions made by silicon and fly ash, it can be found that the chemical constituents of the three aforementioned materials are CaO [or Ca (OH)2, as a gas concretion], β-C2S, and C2AS (the hydraul concretion). The concretions made by these materials have similar flexible wave speeds and suitable congeal speeds (at beginning and end), strong durability of freezing-thawing resistance, water stability, durability of alkali, and durability against changing temperature and humidity. Meanwhile, the porosity of the concretions of the three materials is large, and the concretions exhibit good penetration for gas and water and good compatibility, which makes them ideal conservation materials for repairing the plaster of ancient tomb paintings.%通过对烧料礓石、烧阿嘎土和欧洲水硬石灰 NHL5矿物成分及这三种胶凝材料分别与石英砂、粉煤灰做填料的浆液结石体物理力学特性的分析对比,发现烧料礓石、烧阿嘎土、水硬石灰 NHL5的化学组成主要是气性胶凝材料石灰 CaO(或 Ca(OH)2)和水硬性胶凝材料β-硅酸钙(β-C2S)及铝硅酸钙(C2AS)。试验研究表明,这些材料的结石体有相近的弹性波速和适宜的初凝速度及终凝速度,有强的抗冻融性、水稳定性、耐碱性介质及耐温湿度变化对其强度的影响性。同时,三种胶凝材料结石体孔隙率大,既有好的透气、透水性,又有好的与岩土文物本体结合的兼容性,适宜做古代墓室壁画地仗的修复加固材料。

著录项

  • 来源
    《敦煌研究》|2016年第2期|108-116|共9页
  • 作者单位

    国家古代壁画与土遗址保护工程技术研究中心;

    甘肃 敦煌 736200;

    敦煌研究院;

    甘肃 敦煌 736200;

    中国文化遗产研究院;

    北京 100029;

    国家古代壁画与土遗址保护工程技术研究中心;

    甘肃 敦煌 736200;

    敦煌研究院;

    甘肃 敦煌 736200;

    国家古代壁画与土遗址保护工程技术研究中心;

    甘肃 敦煌 736200;

    敦煌研究院;

    甘肃 敦煌 736200;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 K854.3;
  • 关键词

    料礓石; 阿嘎土; 水硬石灰; 壁画; 地仗; 修复;

  • 入库时间 2022-08-18 01:01:41

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号