某低品位复杂难选黑白钨矿矿物共生关系密切,嵌布粒度细,矿石性质差异性大,获得较好的技术指标较难.分别采用“磁-浮”黑钨白钨分类浮选选矿工艺和“浮-磁-浮”白钨优先浮选选矿工艺对该矿石进行选矿研究.“磁-浮”黑钨白钨分类浮选选矿工艺可获得品位72.59%,回收率30.15%的白钨精矿和品位55.36%,回收率47.81%的黑钨精矿,钨总回收率77.96%.“浮-磁-浮”白钨优先浮选选矿工艺获得WO3品位74.57%、回收率72.90%的白钨精矿和WO3品位28.88%、回收率8.48%的黑钨精矿,钨总回收率为81.38%.%A complex and low grade wolframite-scheelite associated ore has the characteristics of fine granularity and complex embedded relations. It is difficult to obtain good technical indicators. We researched different processes, including magnetic separation-flotation process and flotation- magnetic separation-flotation process, to obtain good technical indicators. By means of magnetic separation-flotation process, scheelite concentrate with grade of 72.59 % WO3 and recovery rate of 30.15 % > and wolframite concentrate with grade of 55.36 % WO3 and recovery of 47.81% > were obtained with the total tungsten recovery rate amounting to 77.96 %. By means of flotation- magnetic separation-flotation process, scheelite concentrate with grade of 74.57 % WO3 and recovery of 72.90 % >and wolframite concentrate with grade of 28.88 % WO3 and recovery of 8.48 %, were obtained with the total tungsten recovery rate amounting to 81.38 %.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号