Synthesis and Characterization of WO3 Loaded TiO2 Nanotube Arrays Electrode and Its Photocatalytic Activity

机译:WO3负载TiO2纳米管阵列电极的合成,表征及其光催化活性。

获取原文
获取原文并翻译 | 示例

摘要

WO3 loaded TiO2 nanotube arrays electrode was prepared by cathodic electrodepositing WO3 onto TiO2 nanotube arrays substrate under square waveform pulses,and the substrate was obtained by potentiostaticanodization of Ti in aggressive media(NH4 F,H2 O,and Glycerol).The solution for electrodepositing consists in a mixture of 5 mM Na2 WO4,20 mM H2 O2 and 70 mL 40% isopropanol solution acidified at pH 1.2 by perchloric acid addition.Square waveform pulses were applied on the substrate with cathodic pulse potentials of-0.24 V vs SCE for WO3 deposition,with the pulse duration of 100 ms,followed by a potential pulse at 0 V for 1000 ms.
机译:通过在矩形波脉冲下将WO3阴极电沉积到TiO2纳米管阵列基板上制备WO3负载的TiO2纳米管阵列电极,并通过在侵蚀性介质(NH4 F,H2 O和甘油)中对Ti进行恒电位阳极氧化来获得基板。在5 mM Na2 WO4、20 mM H2 O2和70 mL 40%异丙醇溶液(通过加入高氯酸酸化)中混合成酸性,在pH 1.2时酸化。在阴极上施加方波脉冲,阴极电位为-0.24 V vs SCE,用于WO3沉积,脉冲持续时间为100 ms,随后是0 V的潜在脉冲持续1000 ms。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号