Development of Cement Compositions with a Finely Dispersed Additive for Consolidation of Soil by the Injection

机译:用精细分散的添加剂进行水泥组合物,用于通过注射固结土

获取原文

摘要

Cement compositions prepared by mixing cement with a stabilized finely dispersed slag suspension, which allow improving the structural, physical and mechanical characteristics of the cement stone are considered. On the first day of hardening, the strength of modified specimens increased by 54%, at the grade age - by 43%, and the porosity decreased by 13.8 and 17.3%, respectively. The possibility of obtaining an injection solution for soil consolidation on the basis of Portland cement and a stabilized slag suspension with the concentration of a finely dispersed slag of 50 g/l is considered. Studies have shown that the injection solution under study has reduced viscosity and sedimentation, increased compressive strength. After 28 days of hardening, the strength was 14.2 MPa, which is higher than the recommended values for consolidation of soil under the foundations (4-6 MPa), and at a concentrated load, for the base under the foundations of the columns (9-10 MPa). The data obtained allows considering an injection solution based on Portland cement and slag suspension for the use in the injection technology of soil consolidation.
机译:通过将水泥与稳定的细散分散的炉渣悬浮液混合来制备的水泥组合物,其允许改善水泥石的结构,物理和机械特性。在硬化的第一天,改性标本的强度增加了54%,等级为43%,孔隙率分别降低了13.8%和17.3%。考虑了在波特兰水泥基础上获得土壤固结的注射液的可能性,并考虑了具有50g / L的细分散渣的浓度的稳定炉渣悬浮液。研究表明,研究的注射溶液具有降低粘度和沉降,抗压强度增加。在28天后,强度为14.2MPa,其高于建议在基础(4-6MPa)下固结土壤的推荐值,并且在柱基础下的浓缩载荷(9 -10 MPA)。所获得的数据允许考虑基于波特兰水泥和炉渣悬架的注射解决方案,用于土壤固结的注射技术。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号