Aggregate impact value (AIV) of fly ash geopolymer artificial aggregate at different sodium hydroxide (NaOH) concentration

机译:不同氢氧化钠(NaOH)浓度的粉煤灰地质聚合物人工骨料的聚集抗冲值(AIV)

获取原文

摘要

This research was conducted to study the aggregate impact value (AIV) of fly ash geopolymer artificial aggregate at different sodium hydroxide (NaOH) concentration. This research involves five different concentrations of NaOH solution which are 6M, 8M, 10M, 12M and 14M while ratio of NaOH/NaSi_2O_3 is constant at 2.5. In this study, the ratio of solid to liquid is fix at 3.0. The characterization of fly ash was observed by Scanning Electron Microscope (SEM). Results show that, the sample with 12M of NaOH concentration give the lowest percentage of AIV (22.43%) which denotes a high performance of aggregate in concrete field and also contribute to high performance of concrete while 6M of NaOH concentration gives the highest percentage of AIV (26.95%). The tested results indicated that the significant potential of fly ash geopolymer aggregate as an alternative artificial aggregate in construction materials field.
机译:进行该研究以研究不同氢氧化钠(NaOH)浓度的粉煤灰地质聚合物人工骨料的聚集抗冲击值(AIV)。 该研究涉及五种不同浓度的NaOH溶液,其为6m,8m,10m,12m和14m,而NaOH / Nasi_2O_3的比例在2.5时恒定。 在该研究中,固体与液体的比例在3.0时固定。 通过扫描电子显微镜(SEM)观察粉煤灰的表征。 结果表明,具有12M的NaOH浓度的样品,其AIV(22.43%)的最低比例(22.43%)表示混凝土领域的高性能,并且还有助于高性能的混凝土,而6M NaOH浓度占AIV的最高百分比 (26.95%)。 测试结果表明,粉煤灰地质聚合物骨料作为建筑材料领域中的替代人为骨料的显着潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号