Influence of Hot Deformation on Microstructure of Non-quenching and Non-tempering Pipe 36Mn2V Used in Oil Well

机译:热变形对油井中使用的非淬火和非回火管36Mn2V微观结构的影响

获取原文

摘要

The continuous rolling and sizing processes for producing non-quenching and non-tempering 36Mn2V steel pipes used in oil well were studied by the thermomechanical simulation test in this paper. The results showed clearly that the final microstructure was influenced by deformation temperature and stain applied. When continuous rolling temperature was controlled at 1050° C and strain at about 0.5 or above, dynamic recrystallization was completed and fine austenitic grain was obtained. When sizing temperature was controlled at 850° C or below and strain at about 0.2 or above, fine acicular ferrite was obtained with properties satisfying the requirement of the high quality pipe. The results of the study provided reliable data for the controlled rolling and sizing processes for the production of the 36Mn2V steel pipes.
机译:通过本文的热机械模拟试验研究了用于油井中使用的非淬火和非回火36Mn2V钢管的连续轧制和施胶方法。 结果表明,最终的微观结构受变形温度和染色的影响。 当在1050℃并在约0.5或更高的菌株下控制连续轧制温度时,完成动态重结晶并获得细细的奥氏体晶粒。 当施胶温度在850℃或更低控制时,在约0.2或更高的菌株下,用满足高质量管道要求的性能获得精细的针状铁氧体。 该研究的结果为生产36Mn2V钢管生产的受控轧制和施胶工艺提供了可靠的数据。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号