Results of an experimental investigation on bond between thermally conditioned FRCM-masonry joints is presented and discussed in the paper. Single lap shear tests were conducted on clay brick specimens strengthened with different FRCM systems (basalt, steel and PBO-FRCM systems). Before testing specimens were thermally conditioned by exposure to different temperature values: 20°C (ambient temperature), 100 °C, 150 °C and 200°C. The thermal treatment was developed in this way: strengthened specimens were kept in oven and exposed to constant temperature over a period of three hours, then, they were removed and cooled down freely to ambient temperature. After the thermal treatment, specimens were tested at ambient temperature. Experimental results allow to evaluate the influence of the thermal conditioning on the local bond-slip response of strengthened specimens.
机译:提出并讨论了热调节的FRCM-砌体关节之间键的实验研究结果。在用不同FRCM系统(玄武岩,钢和PBO-FRCM系统)加强的粘土砖样品上进行单圈剪切试验。在测试试样通过暴露于不同的温度值来热调节:20℃(环境温度),100℃,150℃和200℃。以这种方式开发出热处理:将加强的标本保持在烘箱中并在三小时内暴露于恒定温度,然后除去它们,并自由地冷却至环境温度。在热处理后,在环境温度下测试样品。实验结果允许评估热调节对加强标本局部粘结响应的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号